首页|Characterization and analysis of non-metallic inclusions in Ni42–Fe expansive alloy
Characterization and analysis of non-metallic inclusions in Ni42–Fe expansive alloy
扫码查看
点击上方二维码区域,可以放大扫码查看
原文链接
NETL
Cracks and ruptures always occur during wire drawing process of 42% nickel-iron expansive alloy.In order to study the reasons of these phenomena,a method of metallographic observation in combination with sample electrolysis was used to characterize the non-metallic inclusions in the alloy wire.The results indicate that the inclusions in the alloy are oxidation products during the process of melting.There are single or complex phase inclusions composed of elements such as Al,Si,Ca,Ti,Fe,and O2.Among them,the macro-inclusions are TiO2 compound inclusions formed by the adhesion of Al and Si oxides on them.These inclusions are fragile ones with a low strain rate,as well as a rather high hardness,so that they are the main reason that leads to the surface cracks and ruptures in the alloy wires.The analysis has educed that the key point to enhance the product quality is to promote the cleanliness of the melt,control the types and quantity of non-metal inclusions in the alloy.
non-metallic inclusionscharacterizationanalysis
YAO Ying、OU Guoli
展开 >
SHEN Jie@Key Laboratory of Non-ferrous Metal Alloys,The Ministry of Education,Lanzhou University of Technology,Lanzhou 730050,China
Jinchuan Nickel and Cobalt Research and Engineering Institute,Jinchuan Group Ltd.,Jinchang 737100,China--XIA Tian-dong@Key Laboratory of Non-ferrous Metal Alloys,The Ministry of Education,Lanzhou University of Technology,Lanzhou 730050,China
ICNFM 2007;International Workshop on Nonferrous Materials
Changsha and Zhangjiajie(CN)
Transactions of Nonferrous Metals Society of China pt.II A