首页|90t转炉冶炼低碳含铝钢脱氧合金化实践

90t转炉冶炼低碳含铝钢脱氧合金化实践

扫码查看
针对90t转炉冶炼低碳含铝钢时合金收得率低的问题,分析了影响合金收得率的主要原因,采取优化转炉终点钢水中的氧含量,优化复合脱氧合金配比,调整渣料组成并合理使用挡渣塞后,降低了脱氧铝的消耗,合金收得率提高至87.4%,整体合金成本降低7元/t以上.
Practice of Alloying Operation after Deoxidizing for Low Carbon Aluminum-Containing Steel by 90t Converter
Aiming at the problem that the alloy yield was low in smelting the low carbon alu-minum-containing steel by 90t converter,the main causes leading to the low alloy yield were an-alyzed. After optimizing the content of oxygen in molten steel at the end point and the ratio of al-loying after deoxidizing,adjusting the compositions in slag and applying the slag stopper reason-ably,the consumption of deoxidized aluminum was reduced and the alloy yield was increased to 87.4% and therefore the total cost for alloy was reduced by more than 7 yuan per ton.

converterlow carbon aluminum-containing steelalloying after deoxidizingalloy yield

赵帅、臧绍双、罗建华、王刚、侯永胜

展开 >

鞍钢股份有限公司炼钢总厂,辽宁 鞍山 114021

转炉 低碳含铝钢 脱氧合金化 合金收得率

2024

鞍钢技术
鞍钢技术中心

鞍钢技术

影响因子:0.202
ISSN:1006-4613
年,卷(期):2024.(5)