针对某用户高性能建筑结构用钢SN400B的技术条件,并结合该钢种的高要求应用场合,进行了成分、热轧工艺设计,分析优化出炉温度、终轧温度、卷取温度、终轧与卷取温度差及层流冷却模式等参数,得出结论:较高的出炉温度可以提高强度却不利于延伸率提升;终轧与卷取温度差越大,强度越高,延伸率越低;密集冷却会造成强度较高而塑性较低,一般冷却可得到强度和塑性较佳的综合性能.
Research on hot rolling process of SN400B steel used for high-performance building structure
In light of the technical conditions of SN400B steel used for high performance building structure of a certain user,and in combination with the high demand application of this steel,the composition and hot rolling process design were carried out.Key parameters such as the baking temperature,the final rolling temperature,the coiling temperature,the temperature difference between final rolling and coiling and the laminar cooling mode were analyzed and optimized.It is concluded that:①higher temperature can improve the strength but not the elongation;②the larger the temperature difference between final rolling and coiling,the higher the strength and the lower the elongation;③intensive cooling results in higher strength and lower plasticity,whereas general cooling provides a balanced performance between strength and plasticity.

steel used for high-performance building structureSN400Bcoolingyield ratioelongation at break

高兴健、郑丽婷、杨峰

展开 >

宝钢湛江钢铁有限公司制造管理部,广东湛江 524000

建筑结构用钢 SN400B 冷却 屈强比 断裂延伸率

2024

宝钢技术
宝钢集团有限公司

宝钢技术

影响因子:0.232
ISSN:1008-0716
年,卷(期):2024.(3)
  • 7