材料科学技术(英文版)2021,Vol.71Issue(12) :169-176.

Analysis on fluid permeability of dendritic mushy zone during peritectic solidification in a temperature gradient

Peng Peng Jinmian Yue Anqiao Zhang Xudong Zhang Yuanli Xu
材料科学技术(英文版)2021,Vol.71Issue(12) :169-176.

Analysis on fluid permeability of dendritic mushy zone during peritectic solidification in a temperature gradient

Peng Peng 1Jinmian Yue 1Anqiao Zhang 1Xudong Zhang 1Yuanli Xu1
扫码查看

作者信息

  • 1. Institute of Materials Science and Engineering, Lanzhou University, Lanzhou, 730000, China;School of Physical Science and Technology, Lanzhou University, Lanzhou, 730000, China
  • 折叠

Abstract

Compared with the growing applications of peritectic alloys,none research on the fluid permeability K of dendritic network during peritectic solidification has been reported before.The fluid permeability K of dendritic network in the mushy zone during directional solidification of Sn-Ni peritectic alloy was investigated in this study.Examination on the experimental results demonstrates that both the temperature gradient zone melting (TGZM) and Gibbs-Thomson (G-T) effects have obvious influences on the morphology of dendritic network during directional solidification.This is realized through different stages of liquid diffusion within dendritic mushy zone by these effects during directional solidification.The TGZM effect is demonstrated to play a more important role as compared with the G-T effect during directional solidification.Besides,it is shown that the evolution of dendrite network is more complex during peritectic solidification due to the involvement of the peritectic phase.Through the specific surface Sv,analytical expression based on the Carman-Kozeny model was proposed to analyze the fluid permeability of dendritic mushy zone in directionally solidified peritectic alloys.In addition,it is interesting to find a rise in permeability K after peritectic reaction in both theoretical predication and experimental results,which is different from that in other alloys.The theoretical predictions show that this rise in fluid permeability K after pedtectic reaction is caused by the remelting/resolidification process on dendritic structure by the TGZM and G-T effects during peritectic solidification.

Key words

Alloys/Diffusion behaviour/Directional solidification/Peritecticm icrostructures/Solid/liquid interface

引用本文复制引用

基金项目

project from the Natural Science Foundation of China(51871118)

2018 Joint Foundation of Ministry of Education for Equipment Pre-research(6141A020332)

Key Research and Development Plan of Gansu Province(18YF1GA102)

Fundamental Research Funds for the Central Universities(lzujbky-2019-sp03)

fund of Science and Technology Project of Lanzhou City(2019-1-30)

fund of State Key Laboratory of Special Rare Metal Materials(SKL2020K003)

出版年

2021
材料科学技术(英文版)
中国金属学会 中国材料研究学会 中国科学院金属研究所

材料科学技术(英文版)

CSTPCDCSCDSCI
影响因子:0.657
ISSN:1005-0302
参考文献量36
段落导航相关论文