为了使硫化镍钴(NiCo2S4)作为超级电容器电极材料获得更高的倍率性能和循环稳定性,添加葡萄糖,通过水热法在核心NiCo2S4上涂覆导电碳层,制备NiCo2S4@C.碳层可以防止NiCo2S4聚集,形成更多的微孔,从而形成相对较大的比表面积.所制备的NiCo2S4@C显示出较好的倍率性能,在1 Ag-1时的比电容为1587.8 Fg-1,最高可达1162.5 Fg-1(10 Ag-1).此外,其容量保持率在2000次循环后高达96.2%.
Preparation of Modified NiCo2S4@C Materials Suitable for Supercapacitor Electrodes by One-Pot Solvothermal Method
In order to obtain higher multiplicity performance and cycling stability of nickel cobalt sulfide (NiCo2S4) as supercapacitor electrode material, NiCo2S4@C was prepared by hydrothermally coating a conductive carbon layer on the core NiCo2S4 with the addition of glucose, which prevented the aggregation of NiCo2S4 and formed more micropores, resulting in a relatively large specific surface area. The prepared NiCo2S4@C showed a good multiplicative performance with a specific capacitance of 1587.8 Fg-1 at 1 Ag-1 and up to 1162.5 Fg-1 (10 Ag-1). In addition, its capacity retention rate was 96.2% after 2000 cycles.

NiCo2S4rate performancecycle stabilitysupercapacitorcoating carbon

汪博、路云帆、李小兰、张立磊

展开 >

南华大学 化学化工学院,湖南衡阳 421001

NiCo2S4 倍率性能 循环稳定性 超级电容器 涂层碳

2024

电工材料
桂林电器科学研究院

电工材料

影响因子:0.378
ISSN:1671-8887
年,卷(期):2024.(2)
  • 9