研究了卫材用生物降解外包膜在85℃、85%相对湿度条件下的湿热老化性能,以及在70℃水煮条件下卫材用生物降解外包膜专用料熔体流动速率变化趋势。结果表明,湿热老化对外包膜的拉伸强度的影响大于断裂伸长率;加入1%聚合型抗水解剂湿热老化性能保持率效果最好,拉伸强度保持率在70%以上,断裂伸长率保持率在100%以上,即使抗水解剂加入量明显减少的情况下,外包膜的抗湿热老化性能表现依旧优异;膜材料体系熔体质量流动速率变化越小,湿热老化性能保持率越好。
Study on Hygrothermal Aging of Biodegradable Coating for Sanitary Ware
Absrtact:The aging properties of eisai biodegradable coating at 85 ℃ and 85%humidity were studied.The changing trend of melt flow rate of eisai biodegradable coating was studied at 70 ℃.The results show that the effect of moisture-heat aging on tensile strength is greater than that of elongation at break.The addition of 1%polymerized antihydrolytic agent has the best effect on moisture-heat aging retention,the tensile strength retention is above 70%,and the elongation at break retention is above 100%.Even if the addition amount is significantly reduced,the resistance to moisture-heat aging is still excellent.The smaller the change of melt mass flow rate of membrane material system,the better the retention rate of moisture and heat aging property.

eisaibiodegradationmoisture and heat aging

谢重振、黎万丽、丁建萍、宿鹏、杨文贤、郭志成

展开 >

新疆蓝山屯河高端新材料工程技术研究中心有限公司,新疆昌吉 831100

新疆维格瑞生物科技有限公司,新疆昌吉 831100

卫材 生物降解 湿热老化

新疆维吾尔自治区重点研发计划

2022B1032-4

2024

合成材料老化与应用
广州合成材料研究院

合成材料老化与应用

CSTPCD
影响因子:0.279
ISSN:1671-5381
年,卷(期):2024.53(3)