塔吉克斯坦某含砷金精矿金品位73.27 g/t、砷品位6.61%、硫品位16.78%,是典型的难处理金精矿,采用直接氰化炭浆工艺处理时,金浸出率仅为88.02%.为提高金浸出率,进行含砷金精矿两段焙烧—浸出试验研究,制得的焙砂使用环保型浸出剂浸出.最终得到浸渣金品位4.32 g/t,金浸出率95.43%的良好指标,金浸出率提高7.41百分点,对处理同类型金矿资源起到指导作用.
Experimental study on two-stage roasting-leaching of arsenic-bearing gold concentrate in Tajikistan
The arsenic-bearing gold concentrate in Tajikistan has typical characteristics of refractory gold concen-trate,with a gold grade of 73.27 g/t,arsenic grade of 6.61%,and sulfur grade of 16.78%.When treated with direct cyanidation CIP process,the gold leaching rate was only 88.02%.In order to improve the gold leaching rate,experimental studies on two-stage roasting-leaching of arsenic-bearing gold concentrate were conducted,and the roasted slag was leached using the environmentally friendly leaching agent.The final results showed a good indicator of the gold grade in the leached residue at 4.32 g/t,with a gold leaching rate of 95.43%.This represents an increase of 7.41 percentage points compared to the direct cyanidation CIP process.The study provides guidance for the processing of similar types of gold ore resources.

gold concentrateroastingleaching rateenvironmentally friendly leaching agentarsenicsulfur

余鹤雷、王闯、高起鹏、马忠臣、徐耀强

展开 >

沈阳有色金属研究院有限公司

金精矿 焙烧 浸出率 环保浸出剂

2024

黄金
长春黄金研究院

黄金

CSTPCD
影响因子:0.446
ISSN:1001-1277
年,卷(期):2024.45(2)
  • 11