针对青海某铜铅锌多金属矿,进行了不同类型捕收剂对铜铅锌浮选分离影响的试验,重点考察了新型捕收剂4037B、P5100C、QBSC的选别效果.结果表明:P5100C和QBSC更有利于铜、铅分离,在最佳条件下,采用铜快速浮选—铜铅混选—铜铅再磨分离—锌浮选流程,获得铜品位35.56%、铜回收率75.23%的铜精矿;铅品位 45.02%、铅回收率 71.92%的铅精矿;锌品位41.49%、锌回收率72.58%的锌精矿;含铜 20.14%、含铅 8.90%、含锌 28.38%,铜回收率11.93%、铅回收率6.77%、锌回收率11.81%的混合精矿.全流程铜总回收率97.94%,铅总回收率96.62%,锌总回收率92.64%.
Research on the ore-dressing technology of a copper-lead-zinc polymetallic mine in Qinghai
This study investigates the effects of different types of collectors on the flotation separation of copper,lead,and zinc in a polymetallic mine in Qinghai.The emphasis was placed on evaluating the separation efficiency of new types of collectors 4037B,P5100C,and QBSC.The results indicate that P5100C and QBSC are particularly effec-tive for the separation of copper and lead.Under optimal conditions,a process comprising rapid flotation of copper-mixed flotation of copper and lead-regrinding and separation of copper and lead-zinc flotation,yielded a copper concentrate with a grade of 35.56%and a recovery rate of 75.23%,a lead concentrate with a grade of 45.02%and a recovery rate of 71.92%,and a zinc concentrate with a grade of 41.49%and a recovery rate of 72.58%.A mixed concentrate was also obtained with copper grades of 20.14%,lead grades of 8.90%,zinc grades of 28.38%,and recovery rates of 11.93%,6.77%,and 11.81%for copper,lead,and zinc,respectively.The overall copper,lead,and zinc recovery rates were 97.94%,96.62%,and 92.64%,respectively.

copperleadzincnew types of collectorsflotationpolymetallic mine

赵玉卿、刘氘、张培青、应永朋

展开 >

青海省地质矿产测试应用中心

青海省第三地质勘查院

新型捕收剂 浮选 多金属矿

青海省昆仑英才·高端创新创业人才领军人才项目

青人才字[2021]13号

2024

黄金
长春黄金研究院

黄金

CSTPCD
影响因子:0.446
ISSN:1001-1277
年,卷(期):2024.45(5)
  • 8