混凝土表面点状爆裂问题案例分析

扫码查看
文中针对某项目混凝土表面出现大面积点状爆裂现象,通过现场取样对病害部位混凝土进行强度体积稳定性和X射线荧光成分分析(XRF))等项目检测和分析,结果表明,病害部位存在游离氧化钙(f-CaO)的潜在危害,而f-CaO较大可能是不合格钢渣所致.
Case Analysis of Single Point Burst on Concrete Surface
A large area of concrete surface point like cracking occurred in a certain project's concrete structure.Through on-site sampling,strength volume stability and X-ray fluorescence composition analysis(XRF)tests were conducted on the affected concrete.The results showed that there is a potential danger of free calcium oxide in the affected area,and the large amount of free calcium oxide may be caused by the use of unqualified steel slag in the concrete.

ConcretePoint burstFree calcium oxideSlag