科技和产业2024,Vol.24Issue(24) :333-340.

盾构泥饼同步注浆浆液的制备与性能分析

Preparation and Performance Analysis of Synchronized Grouting Slurry for Shield Mud Cake

匡建军 张光伟 林四新 张伟
科技和产业2024,Vol.24Issue(24) :333-340.

盾构泥饼同步注浆浆液的制备与性能分析

Preparation and Performance Analysis of Synchronized Grouting Slurry for Shield Mud Cake

匡建军 1张光伟 1林四新 2张伟3
扫码查看

作者信息

  • 1. 中国交建轨道交通分公司,北京 101300
  • 2. 中交三航局第六工程(厦门)有限公司,福建厦门 361021
  • 3. 福建理工大学,福州 350118
  • 折叠

摘要

为推动盾构渣土的资源化再利用和无害化处理,对盾构泥饼的微观性能和基本物理性能进行分析,确定了盾构泥饼可作为注浆材料中膨润土、粉煤灰、细砂的替代物的方案,并进行抗压强度、凝结时间、泌水率和流动度试验.结果表明,当泥饼替代膨润土时,可有效改善同步注浆浆液性能,且最佳同步注浆材料水泥、粉煤灰、细砂、水、膨润土、泥饼的配比为 1∶2.71∶2.61∶3.42∶0.49∶0.16.

Abstract

In order to promote the recycling and harmless disposal of shield tunneling muck,the microscopic and basic physical properties of shield mud cakes were analyzed,the programme wich that they can be used as substitutes for bentonite,fly ash and fine sand in grouting materials was determined.The compressive strength,setting time,bleeding rate,and fluidity of grouting slurries with different substitution rates of shield mud cakes were analyzed.The research results indicate that when mud cakes are used as a substitute for bentonite,the bleeding rate improves,while fluidity and setting time remain relatively stable.The optimal ratio of cement,fly ash,fine sand,water,bentonite and mudfor synchronous grouting materials is 1∶2.71∶2.61∶3.42∶0.49∶0.16.

关键词

盾构泥饼/微观性能/抗压强度/凝结时间/泌水率/流动度

Key words

shield mud cake/microscopic properties/compressive strength/setting time/bleeding rate/fluidity