首页|侧吹炉协同处理铜阳极泥浸出渣回收有价金属新工艺研究

侧吹炉协同处理铜阳极泥浸出渣回收有价金属新工艺研究

扫码查看
采用侧吹炉协同处理铜阳极泥浸出渣,综合回收有价金属,考察了纯碱用量、粒煤用量、沉淀时间、炉顶烟气温度对主金属Pb、Sb、Bi、Au、Ag回收率的影响.结果表明,适宜的处理工艺参数为:纯碱用量2.5%、粒煤用量3%、沉淀时间1.5 h、炉顶烟气温度750 ℃,此时贵铅中Au品位达到1 544 g/t(富集了 1.84倍)、Ag品位达到10.37%(富集了 1.4倍)、Pb品位达到22.89%(富集了 2.1倍)、Bi品位达到27.45%(富集了 2.2倍).
A New Process for Recovering Valuable Metals from Leaching Residue of Copper Anode Slime by Side Blowing Furnace
A side blowing furnace was adopted to treat the leaching residue of copper anode slime and recover valuable metals therein comprehensively.The effects of soda dosage,granular coal dosage,precipitation time and top flue gas temperature on the recovery rates of main metals Pb,Sb,Bi,Au and Ag were investigated.The results show that with soda at an amount of 2.5%,granular coal at an amount of 3%,the precipitation time of 1.5 h,and the top flue gas temperature of 750 ℃,the precious lead product is obtained after processing,grading 1 544 g/t Au(1.84 times enrichment),10.37%Ag(1.4 times enrichment),22.89%Pb(2.1 times enrichment),and 27.45%Bi(2.2 times enrichment).

side blowing furnacecopper anode slimeleaching residuerare and precious metalsvaluable metalsenrichmentleadantimonybismuthgoldsilver

闫友

展开 >

湖南水口山有色金属集团有限公司,湖南衡阳 421513

侧吹炉 铜阳极泥 浸出渣 稀贵金属 有价金属 富集

国家重点研发计划

2018YFC1903300

2024

矿冶工程
长沙矿冶研究院有限责任公司 中国金属学会

矿冶工程

CSTPCD北大核心
影响因子:1.137
ISSN:0253-6099
年,卷(期):2024.44(1)
  • 12