首页|低品位高滑石型钼矿高效分离工艺研究

低品位高滑石型钼矿高效分离工艺研究

扫码查看
针对河南某高滑石型难选辉钼矿脱泥流程中钼损失量大、钼和滑石分离困难的问题,在脱泥工艺中添加一定的ZN-J1 有效降低了辉钼矿在脱泥工段中的损失,以水玻璃+ZN-P1作为分离工艺的组合抑制剂,在原矿Mo品位0.116%、硫化钼占比 83.53%、滑石相对含量 14.0%条件下,采用"脱泥-钼预浮选-再磨-钼与滑石分离"的工艺流程,全流程闭路试验得到了钼精矿品位 47.68%、钼回收率 75.41%的优良指标.
Efficient Separation Process for Low-Grade High-Talc Molybdenum Ore
In response to the problems of high molybdenum loss and difficulty in molybdenum/talc separation existing in the desliming process of a high talc-type molybdenite ore from Henan,ZN-J1,a molybdenum depressant,was introduced in the desliming section to minimize efficiently the molybdenum loss.The feed ore with Mo grade of 0.116%,molybdenum sulfide percentage of 83.53%and talc content of 14.0%was processed by adopting a flowsheet,consisting of desliming,pre-flotation of molybdenum,regrinding,and molybdenum/talc separation,with a combination of sodium silicate and ZN-P1 as depressant.A closed-circuit test with the whole process produced a molybdenum concentrate with Mo grade of 47.68%and Mo recovery of 75.41%,respectively.

molybdenitetalcdeslimingdepressant

吴奕彤、焦芬、魏茜、蒋素芳

展开 >

中南大学 资源加工与生物工程学院,湖南 长沙 410083

辉钼矿 滑石 脱泥 抑制剂

国家自然科学基金面上项目

51974364

2024

矿冶工程
长沙矿冶研究院有限责任公司 中国金属学会

矿冶工程

CSTPCD北大核心
影响因子:1.137
ISSN:0253-6099
年,卷(期):2024.44(2)