矿冶工程2024,Vol.44Issue(3) :73-76.DOI:10.3969/j.issn.0253-6099.2024.03.016

某冶金级萤石精矿提质降杂试验研究

Experimental Study on Improving Quality and Reducing Impurities of Metallurgical Grade Fluorite Concentrate

冯青舒 缪亚兵 陈文胜 刘旭 王舰 李文风 赵文坡 陆泽雍
矿冶工程2024,Vol.44Issue(3) :73-76.DOI:10.3969/j.issn.0253-6099.2024.03.016

某冶金级萤石精矿提质降杂试验研究

Experimental Study on Improving Quality and Reducing Impurities of Metallurgical Grade Fluorite Concentrate

冯青舒 1缪亚兵 2陈文胜 3刘旭 2王舰 3李文风 2赵文坡 2陆泽雍2
扫码查看

作者信息

  • 1. 湖南柿竹园有色金属有限责任公司,湖南 郴州 423037
  • 2. 长沙矿冶研究院有限责任公司,湖南长沙 410012
  • 3. 湖南有色郴州氟化学有限公司,湖南 郴州 423037
  • 折叠

摘要

针对某CaF2 品位 70.34%的冶金级萤石精矿进行了提质降杂试验研究.结果表明,采用"强磁选降硅-非磁性产品浮选降钙"工艺,实验室全流程试验获得了精矿产率58.30%、CaF2 品位91.95%、回收率76.52%的萤石产品,萤石产品质量达到了制备无水氢氟酸的原料要求.

Abstract

An experimental study on a metallurgical grade fluorite concentrate with CaF2 content of 70.34%was conducted to upgrade fluorite concentrate quality by reducing impurities therein.The results of the full process test show that by adopting a process of high intensity magnetic separation for reducing silicon,followed by flotation of non-magnetic minerals for reducing calcium,the experiment produces a fluorite concentrate grading of 91.95%CaF2 at 76.52%recovery,with a yield of 58.30%.It is shown that the concentrate meets the raw material standards for anhydrous hydrofluoric acid production.

关键词

萤石/强磁选/浮选/提质降杂/氢氟酸

Key words

fluorite/high intensity magnetic separation/flotation/improving quality and reducing impurities/hydrofluoric acid