为研究潮湿细粒煤复合式干法分选效率,对潮湿细粒煤进行了振动强度和气速的单因素试验,结合RSM-BBD预测模型获得了最优参数;并探索了不同水分的原煤在不同分选时间内的分选效果,同时分析了气流对潮湿细粒煤分选过程的影响,并评价了分选效果.结果表明:随着分选时长的增加,分选效果明显提高,最大灰分离析度可达 12.05.试验煤样在气速为 0.78 m/s,振动频率为25 Hz,振幅为 3 mm时达到最佳分选效果,此时可能偏差E=0.135 g/cm3,且在此条件下分选产品有很好的脱水效果,复合式干法分选可实现潮湿煤炭的提质.该研究可以对细粒煤炭的干法分选工艺提供理论和技术支持.
Separation characteristics of moist fine coal in a compound dry separator
To improve the efficiency of moist fine coal sorting and classification,a single-factor test of vibration intensity and air velocity was carried out in a compound dry separator to obtain the optimal parameters,and the separating effect of raw coal with different moisture in different separating duration was explored,while the influence of airflow on the separating process of moist fine coal was analyzed.The results show that with the increase of separating duration,the separating effect is obviously improved,and the maximum ash segregation degree is up to 12.05.The test coal samples reach the best separation effect at the air velocity of 0.78 m/s,the vibration frequency of 25 Hz,and the amplitude of 3 mm,and the separated products have good dewatering effect at this condition,and the dewatering effect of the concentrate coal is better,the possible deviation E=0.135 g/cm3.And the separated products have good dewatering effect under this condition,and the composite dry sorting can realize the quality enhancement of moist coal.

moist fine coalcompound dry separationash segregation degreedistribution curveresponse surface method

陈存强、顾雷雨、周延明、汪义龙、冯来宏、曹睿、高利晶、刘海涛、唐海龙

展开 >

华能云南滇东能源有限责任公司, 云南 曲靖 655508

华能煤炭技术研究有限公司, 北京 100070

华亭煤业公司砚北煤矿, 甘肃 平凉 744100

中国矿业大学, 江苏 徐州 221116

展开 >

潮湿细粒煤 复合干选 灰分离析度 分配曲线 响应面法

华能集团总部科技项目

HNKJ20-H36

2024

煤炭工程
煤炭工业规划设计研究院

煤炭工程

CSTPCD北大核心
影响因子:0.806
ISSN:1671-0959
年,卷(期):2024.56(5)
  • 29