首页|中南股份50板弯曲率的改善措施及效果

中南股份50板弯曲率的改善措施及效果

扫码查看
中南股份特轧厂3450 mm生产线,在生产40 mm以下规格50板时,出现较多弯曲现象.产线通过加热炉工艺改善、轧制工艺改善、冷却工艺改善、矫直工艺改善等措施,对轧制过程进行优化,有效降低了 50板弯曲率,提高了产品质量.
Study on Improvement Measures and Effects of Plate 50 Bending Rate at Guangdong ZNIS
At present,when plates 50 with thickness below 40 mm are produced,there are much bending phenomena in rolling at Guangdong ZNIS.The rolling line has been optimized by improving the reheating furnace process,rolling process,cooling process and straightening process,which help reduce the bending rate of the plates effectively and improve the product quality.

plate rollingplate 50bending

巫献华、李班、幸岚春、张鑫、邓贤冬

展开 >

宝武集团中南钢铁广东中南钢铁股份有限公司,广东韶关 512123

板材工序 50板 弯曲

2024

南方金属
广东省金属学会

南方金属

影响因子:0.16
ISSN:1009-9700
年,卷(期):2024.(2)
  • 2