首页|6082T6铝合金板搅拌摩擦焊接工艺研究

6082T6铝合金板搅拌摩擦焊接工艺研究

扫码查看
本文主要对3 mm厚6082T6铝合金搅拌摩擦焊接工艺进行研究,研究了轴肩下压量、焊接速度、旋转速度工艺参数对接头组织性能的影响,同时对焊接接头进行了金相、显微硬度、拉伸和弯曲等试验.结果表明3 mm厚度6082T6铝合金板搅拌摩擦焊最优工艺参数为,轴肩下压量0.15 mm、旋转速度1400 r/min、焊接速度1 000 mm/min时,接头焊缝强度系数可达0.82.
Study on friction stir welding technology of 6082T6 aluminum alloy
Microstructure and properties of 3mm-thick 6082T6 aluminum alloy were stud-ied with friction stir welding(FSW)process parameters,namely plunge depth of shoulder,welding speed and rotation speed.The welded joints were also conducted with metallograph-ic,microhardness,tensile,and bending tests.The test results indicate the optimal parame-ters,i.e.plunge depth of shoulder,rotation speed and welding speed are 0.15 mm,1 400 r/min and 1 000 mm/min,respectively.Under this process parameter,the strength coeffi-cient of the joint weld can reach 0.82.

6082T6plunge depth of shoulderrotation speedwelding speed

刘庆永、毛晓东、胡国强、高崇、李英东

展开 >

中铝材料应用研究院有限公司,北京 102209

6082T6 轴肩下压量 旋转速度 焊接速度

2024

轻合金加工技术
中国有色金属加工工业协会轻金属分会

轻合金加工技术

影响因子:0.31
ISSN:1007-7235
年,卷(期):2024.52(6)