摘要

利用手工A-TIG焊对20钢管进行了大钝边打底焊研究.钝边尺寸及装配间隙合理时,在适当工艺参数支持下,可实现活性TIG焊全位置大钝边打底焊接.活性剂作用下熔池表面张力方向的改变是影响A-TIG全位置大钝边打底焊成型的重要因素.平焊位置,内表面张力σ2是平衡向下的重力G与电弧力Fa的重要作用力;立焊位置,内表面张力σ2是平衡水平电弧力Fa主要作用力;仰焊位置,外表面张力σ1与内表面张力σ2是克服重力G的重要作用力.

Abstract

A study was conducted on the large blunt edge root welding of 20 steel pipes using manual A-TIG welding.When the size of the blunt edge and the assembly gap are reasonable,with the support of appropriate process pa-rameters,A-TIG welding with full position large blunt edge root can be achieved.The change in surface tension di-rection of the molten pool under the action of an activator is an important factor affecting the formation of A-TIG full position large blunt edge root welding.In the flat welding position,the inner surface tension σ2 is the important force that balances the downward gravity G and the arc force Fa;At the vertical welding position,the inner surface tension σ2 is the main force that balances the horizontal arc force Fa;At the overhead welding position,the outer surface tension σ1.Internal surface tension σ2 is an important force to overcome gravity G.

关键词

活性TIG焊/大钝边/打底焊/全位置

Key words

A-TIG welding/large blunt edge/root welding/all position

引用本文复制引用

基金项目

2023年甘肃省高校教师创新基金项目(2023B-415)

甘肃省陇南市2022年科技计划项目(2022-S·JH-09)

2021年陇南师范高等专科学校校级教学改革重点项目(JXGG2021009)

出版年

2024
四川冶金
四川省冶金情报标准研究所

四川冶金

影响因子:0.165
ISSN:1001-5108
参考文献量7
段落导航相关论文