首页|盐酸预处理—软锰矿+硫酸协同浸出钼钨矿工艺研究

盐酸预处理—软锰矿+硫酸协同浸出钼钨矿工艺研究

扫码查看
针对国内某公司低品位混合型钨钼矿结构和成分复杂、难浮选且难浸出等问题,研究了盐酸预处理—软锰矿+硫酸协同浸出钼钨矿中的钼钨,考察了各因素对钨钼浸出率的影响.结果表明:在盐酸浓度1.5 mol/L、液固体积质量比6.5/1、常压条件下,对钨钼矿石进行盐酸预处理;在盐酸预处理后滤渣20 g、矿石粒度200目、软锰矿用量4 g、硫酸浓度8 mol/L,液固质量体积比5/1、温度90 ℃、浸出时间3 h的最佳条件下,钼、钨浸出率分别为83%、73%.
Hydrochloric Acid Pretreatment-Pyrolusite+Sulfuric Acid Synergistic Leaching Process of Molybdenum Tungsten Ore
In view of the complex structure,difficult flotation and difficult leaching of low-grade mixed tungsten and molybdenum ore of a domestic company,the synergistic leaching of molybdenum and tungsten from molybdenum tungsten ore by hydrochloric acid pretreatment-pyrolusite+sulfuric acid was studied.The effects of various factors on the leaching rate of tungsten and molybdenum were investigated.The results show that under the conditions of hydrochloric acid concentration of 1.5 mol/L,liquid volume to solid mass ratio of 6.5/1 and atmospheric pressure,the tungsten and molybdenum ores are pretreated with hydrochloric acid.Under the optimal conditions of filter slag of 20 g,particle size of 200 mesh,pyrolusite dosage of 4 g,sulfuric acid of 8 mol/L,liquid volume to solid mass ratio of 5/1,temperature of 90 ℃ and leaching time of 3 h,the leaching rates of molybdenum and tungsten are 83%and 73%,respectively.

molybdenum tungsten orehydrochloric acidpretreatmentpyrolusitesulfuric acidsynergistic leachingmolybdenumtungsten

陶乐、张勤、陈俊英、高瀚杰、刘海鹏、杨洪英

展开 >

东北大学冶金学院,辽宁沈阳 110819

东北大学多金属矿生态冶金重点实验室,辽宁沈阳 110819

钼钨矿 盐酸 预处理 软锰矿 硫酸 协同浸出

2024

湿法冶金
核工业北京化工冶金研究院

湿法冶金

北大核心
影响因子:0.631
ISSN:1009-2617
年,卷(期):2024.43(4)