首页|亚硫酸铵还原焙烧软锰矿提取锰试验研究

亚硫酸铵还原焙烧软锰矿提取锰试验研究

扫码查看
研究了以亚硫酸铵为还原剂,通过高温焙烧直接把软锰矿中的二氧化锰还原成硫酸锰,从而实现软锰矿的高效提取,考察了亚硫酸铵与软锰矿质量比、焙烧温度及时间、浸出温度及时间等对锰提取率的影响,确定了最佳工艺条件.结果表明:最优条件为亚硫酸铵与软锰矿质量比0.75∶1,焙烧温度500 ℃,焙烧时间1.5 h,浸出温度25 ℃,浸出时间30 min;在该条件下,锰浸出率约为93%,铁浸出率约9.5%.锰提取效果较好.
Extraction of Manganese from Manganese Dioxide Ores by(NH4)2SO3 Reduction Roasting
Manganese dioxide in pyrolusite was directly reduced to manganese sulfate by high-temperature roasting with ammonium sulfite as reducing agent,so as to achieve efficient extraction of pyrolusite.The effects of mass ratio of ammonium sulfite to pyrolusite,roasting temperature and time,leaching temperature and time on the extraction rate of manganese were investigated,and the optimum process conditions were determined.The results show that the optimal conditions are the mass ratio of ammonium sulfite to pyrolusite of 0.75∶1,roasting temperature of 500 ℃,roasting time of 1.5 h,leaching temperature of 25 ℃,leaching time of 30 min.Under the conditions,the leaching rate of manganese and iron is about 93%and about 9.5%,respectively.The extraction effect of manganese is good.

pyrolusiteammonium sulfiteroastingreductionleachingextractionmanganeseiron

黎应芬、胡林、王润玺、王志琦

展开 >

贵州理工学院材料与能源工程学院,贵州 贵阳 550003

软锰矿 亚硫酸铵 焙烧 还原 浸出 提取

贵州省教育厅高校科技创新团队

黔教技[2023]078号

2024

湿法冶金
核工业北京化工冶金研究院

湿法冶金

北大核心
影响因子:0.631
ISSN:1009-2617
年,卷(期):2024.43(4)