为满足焊丝生产企业对盘条氧化皮机械剥离性的要求,对轧钢过程中钢坯及盘条表面氧化铁皮成分、特性及结构进行分析,通过采取提高加热炉加热段温度到1 030℃,降低均热温度到1 140 ℃,提高除鳞压力到30MPa,降低吐丝温度、风冷辊道速度和出入保温罩温度等工艺优化措施,改善氧化铁皮的机械剥离性,解决了盘条及中间丝表面氧化铁皮去除不净,镀铜后焊丝外观质量差等问题,保证了氧化铁皮的去除和成品焊丝质量的提高.
Study and Practice on Mechanical Stripping of ER70S-6 Steel for Welding
In order to meet the requirements of welding wire manufacturers for mechanical stripping of wire rod scale,the composition,characteristics and structure of scale on billet and wire rod surface during steel rolling were analyzed.By adopting process optimization measures such as increasing the heating section temperature of heating furnace to 1 030 ℃,reducing soaking temperature to 1 140 ℃,increasing descaling pressure to 30 MPa,reducing spinning temperature,air-cooled roller speed and temperature of entering and leaving the insulation cover,improving the mechanical peeling ability of iron oxide scale,the problems of incomplete removal of iron oxide scale on the surface of wire rods and intermediate wires are solved,as well as poor appearance quality of welding wires after copper plating,ensuring the removal of iron oxide scale and improving the quality of finished welding wires.

iron oxide scalemechanical peelabilityheating temperaturecooling processprocess optimization

吕普明

展开 >

河钢集团宣钢公司技术中心,河北 宣化 075100

氧化铁皮 机械剥离性 加热温度 冷却工艺 工艺优化

2024

山西冶金
山西省金属学会 山西省有色金属学会

山西冶金

影响因子:0.139
ISSN:1672-1152
年,卷(期):2024.47(2)
  • 3