山西冶金2024,Vol.47Issue(3) :24-25,28.DOI:10.16525/j.cnki.cn14-1167/tf.2024.03.009

不同制样方法对焦炭反应性及反应后强度稳定性的研究

Study on the Reactivity and Strength Stability of Coke after Reaction Using Different Sample Preparation Methods

陈鹏
山西冶金2024,Vol.47Issue(3) :24-25,28.DOI:10.16525/j.cnki.cn14-1167/tf.2024.03.009

不同制样方法对焦炭反应性及反应后强度稳定性的研究

Study on the Reactivity and Strength Stability of Coke after Reaction Using Different Sample Preparation Methods

陈鹏1
扫码查看

作者信息

  • 1. 陕钢集团汉钢公司,陕西 汉中 724200
  • 折叠

摘要

焦炭反应性样品制样方式主要有传统的手工制样和机器制样两种,不同的制样方法制出的焦炭颗粒不同,分析了不同焦炭颗粒的稳定性.通过实验研究,得出全自动机械制样焦炭反应性结果稳定,符合实验要求.

Abstract

There are two main methods for preparing coke reactivity samples:traditional manual sample preparation and machine sample preparation.Different sample preparation methods produce different coke particles,resulting in poor stability of analysis results.Through experimental research,it was found that the reactivity results of coke produced by fully automated mechanical sampling are stable and meet the experimental requirements.

关键词

焦炭/反应性/反应后强度/制样/方法/颗粒

Key words

coke/reactivity/post reaction strength/sample preparation/method/granul

引用本文复制引用

出版年

2024
山西冶金
山西省金属学会 山西省有色金属学会

山西冶金

影响因子:0.139
ISSN:1672-1152
参考文献量2
段落导航相关论文