首页|Φ12mm螺纹钢四切分轧制工艺改造实践

Φ12mm螺纹钢四切分轧制工艺改造实践

扫码查看
阳春新钢铁有限责任公司一棒生产线Φ12mm螺纹钢三切分轧制工艺在生产实践中生产效率低,日产仅有2 700 t左右,远低于炼钢1号铸机产能,导致热送热装率较低、能耗浪费较大,且严重制约了公司产能的提升.鉴于此,一棒轧线通过利旧现有设备,成功将Φ12 mm螺纹钢生产工艺由三切分改进为四切分,改造后不仅提升了生产效率,而且切分线差较小、产品精度稳定受控,具有较强的借鉴参考意义.
Practice of Four Section Rolling Process Transformation for Φ12mm Threaded Steel
In the production practice of the three section rolling process of Φ12mm threaded steel for the first bar production line of Yangchun New Iron and Steel Co.,Ltd.,the production efficiency is low,with a daily output of only about 2 700 tons,far lower than the production capacity of the No.1 steelmaking casting machine.This has led to a low hot delivery and charging rate,significant energy waste,and seriously hindered the company's capacity improvement.In view of this,this article introduces the successful improvement of the production process of Φ12mm threaded steel from three cutting to four cutting by utilizing old existing equipment on a rolling line.After the transformation,not only has the production efficiency been improved,but also the cutting line difference is small and the product accuracy is stable and controlled,which has strong reference significance.

four section rolling of Φ12 mm threaded steelhole designrolling programkey control pointscut line difference

谭伟

展开 >

阳春新钢铁有限责任公司,广东 阳春 529600

Φ12mm螺纹钢四切分轧制 孔型设计 轧制程序 控制要点 切分线差

2024

山西冶金
山西省金属学会 山西省有色金属学会

山西冶金

影响因子:0.139
ISSN:1672-1152
年,卷(期):2024.47(10)