首页|硼对金属间化合物Ni3Fe氢气诱发环境氢脆的影响

硼对金属间化合物Ni3Fe氢气诱发环境氢脆的影响

扫码查看
Influence of boron-doping on the H2-induced environmental embrittlement of Ni3Fe intermetallics
In this paper the tensile properties of both ordered and disordered Ni-24Fe and Ni-24Fe-0.03%B (wt%) alloys in gaseous hydrogen was investigated. The result shows that the ductility of the disordered Ni3Fe is significantly larger than that of ordered material in gaseous hydrogen. However, the ductility of ordered Ni3Fe doped with 0.03%B is nearly the same as that of disordered one indicating the obvious suppressing effect of boron on the H2-induced embrittlement. Based on the segregation behavior of boron in Ni3Al, it is proposed that the suppressing effect of boron in Ni3Fe on the H2-induced embrittlement is attributed to the segregation of boron on grain boundaries, thereby reducing the hydrogen diffusivity along the grain boundaries.

hydrogen embrittlement, Ni3Fe alloy, boron addition

石丹丹、陈业新、万晓景、LIU Chain Tsuan

展开 >

Institute of Materials Science, Shanghai University, Shanghai 200072, P. R. China

Department of Materials Science and Engineering, University of Tennessee, TN37996-2200, USA

hydrogen embrittlement, Ni3Fe alloy, boron addition

国家自然科学基金国家自然科学基金

5037105050671057