基于纳米二氧化硅改性下SAP内养护混凝土的基本性能研究

扫码查看
研究纳米二氧化硅(NS)改性SAP内养护混凝土的物理力学性能以及抗氯离子渗透性能,提出该混凝土的配合比设计.复掺0.08%SAP和1.5%NS能提高混凝土抗折强度;复掺0.08%SAP和1.0%NS能提高其抗压强度;复掺0.24%SAP和1.5%NS氣离子抗渗透性能最佳;复掺0.24%SAP和0.5%NS能显著减小干燥收缩率.
Research on the basic properties of SAP internal curing concrete based on nano silica modification
The physical and mechanical properties and chloride ion penetration resistance of nano-silica(NS)modified SAP internal curing concrete are studied,and the mix design of this concrete is put forward.The bending strength of concrete can be improved by adding 0.08%SAP and 1.5%NS.The compressive strength of concrete can be improved by adding 0.08%SAP and 1.0%NS.The per-meability resistance of chloride ion is the best by adding 0.24%SAP and 1.5%NS.Adding 0.24%SAP and 0.5%NS can significantly reduce the drying shrinkage.

nano silica modificationSAP internal curing concretecompressive strengthsetting time

姜佩弦、刘荣桂、张灵灵

展开 >

南通理工学院,江苏南通 226000

纳米二氧化硅 SAP内养护混凝土 标准养护 抗压强度 凝结时间

2018年度国家自然科学基金项目2022年度南通市基础科学研究和社会民生科技计划项目

51778272MSZ2022193

2024

水泥工程
南京水泥工业设计研究院有限公司

水泥工程

影响因子:0.118
ISSN:1007-0389
年,卷(期):2024.(1)
  • 1
  • 15