首页|生产线C5旋风筒入口结皮原因分析

生产线C5旋风筒入口结皮原因分析

扫码查看
某生产线运行期间,5级筒内结皮严重,绝大部分堆积在5级筒入口处,随着烟气旋流向下分布,结皮料中坚硬结皮和疏松结皮均有,颜色有白色和灰色.对结皮进行取样分析,得出结皮产生的主要原因有:(1)原燃料中碱含量偏高;(2)该线分解炉内煤粉燃烧不完全,存在后燃现象,5级筒温度出现倒挂;(3)该系统内,碱含量、氯含量过剩,形成了较多的熔融物质,主要以KCl、K2SO4、CaSO4为主,且KCl含量均在10%以上,极大的降低了熔融物质的液相初析温度,从4级筒开始便出现结皮.
Analysis of the causes of skin formation at the inlet of the C5 cyclone on the production line
During the operation of a production line,the crust in the 5-stage cylinder is serious,and most of it is accumulated at the en-trance of the 5-stage cylinder,and with the downward distribution of the flue gas cyclone,there are both hard crust and crisp crust in the crust material,and the color is white and gray.The main reasons for the formation of crust are as follows:(1)the alkali content in the primary combustion material is high;(2)The combustion of pulverized coal in the decomposition furnace of the line is incomplete,there is aftercombustion,and the temperature of the 5-stage cylinder is inverted;(3)In the system,the alkali content and chlorine con-tent are excessive,and more molten substances are formed,mainly KCl,K2SO4 and CaSO4,and the KCl content is more than 10%,which greatly reduces the initial liquid phase precipitation temperature of the molten substances,and crusting appears from the 4th stage cylinder.

cyclone resistancecrustmolten materialliquid phase initial precipitation temperature

张宗见、张健

展开 >

安徽海螺建材设计研究院有限责任公司,安徽 芜湖 241070

旋风筒阻力 结皮 熔融物质 液相初析温度

2024

水泥工程
南京水泥工业设计研究院有限公司

水泥工程

影响因子:0.118
ISSN:1007-0389
年,卷(期):2024.(3)