首页|HNBR并用量对ACM/HNBR硫化胶力学性能的影响

HNBR并用量对ACM/HNBR硫化胶力学性能的影响

扫码查看
研究了 HNBR并用量对ACM/HNBR硫化胶硫化特性、动态力学性能、物理机械性能、耐低温性的影响.结果表明,当HNBR并用量超过30份后,即可提高共混胶的硫化程度,使得储能模量G'升高,损耗因子tanδ降低;其中,当HNBR并用量为50份时,与纯ACM相比,其老化前拉伸强度提高了 47.9%,拉断伸长率提高了 64.2%,耐磨性提高了 30%,回弹性提高了 88%,此外,HNBR的并用也明显改善了共混胶的抗应力松弛性,明显提高了共混胶老化后拉伸性能.
Effect of HNBR Dosage on Mechanical Properties of ACM/HNBR Vulcanizates
The effects of HNBR dosage on the vulcanization properties,dynamic mechanical prop-erties,physical mechanical properties and low temperature resistance of ACM/HNBR vulcanizates were studied.The results showed that when the HNBR dosage exceeded 30 phr,the vulcanization state of the blend could be improved,the storage modulus G could be increased,and the loss factor tanδcould be decreased.Among them,when the dosage of HNBR was 50 phr,compared with pure ACM.the tensile strength before aging was increased by 47.9%,the elongation at break was in-creased by 64.2%,the wear resistance was increased by 30%,the resilience was increased by 88%,and the low temperature resistance was increased by 65%.In addition,the use of HNBR also signifi-cantly improved the stress relaxation resistance of the blend.The tensile properties of the blend after aging were obviously improved.

HNBRtwo-phase crosslinking densityvulcanization propertymechanical property

刘长顺、代欣、郝良赐、邓涛

展开 >

青岛科技大学高分子科学与工程学院,山东青岛 266042

HNBR 两相交联密度 硫化特性 力学性能

2024

特种橡胶制品
西北橡胶塑料研究设计院

特种橡胶制品

影响因子:0.28
ISSN:1005-4030
年,卷(期):2024.45(6)