为了探究新型钼矿捕收剂MK-01对马坑矿业选铁尾矿回收钼指标的影响,分别使用常规捕收剂煤油和新型钼矿捕收剂MK-01进行实验室试验和工业试验研究.结果表明,在一段磨矿粒度为-0.074 mm占65.38%,再磨粒度为-0.037 mm占83%时,以水玻璃为调整剂,亚硫酸钠+硫酸锌为抑制剂,2#油为起泡剂,采用1粗2精2扫—粗精矿再磨—4次精选流程,以MK-01为捕收剂时,实验室闭路试验可以获得钼品位44.938%、回收率66.54%的钼精矿,相比煤油作捕收剂,钼品位和回收率分别提高了0.636和2.96个百分点;工业试验可以获得钼品位42.26%、回收率62.71%的钼精矿;与煤油为捕收剂时相比,钼品位相近,回收率提高了0.72百分点,捕收剂用量由52 g/t减少到42 g/t.说明新型钼矿捕收剂MK-01可以代替马坑矿业传统钼矿捕收剂煤油使用.
Application Research on a New Type of Molybdenum Collector MK-01 in Separation of Molybdenum of Mackeng Iron Tailings
In order to explore the effect of a new molybdenum collector MK-01 on the recovery index of molybdenum from iron tailings in Makeng Mining,the laboratory test and industrial test of conventional collector kerosene and new molybdenum collector MK-01 were carried out respectively.The results show that when the first-stage grinding particle size is-0.074 mm accounting for 65.38%,and the regrinding par-ticle size is-0.037 mm accounting for 83%,sodium silicate is used as the regulator,sodium sulfite+zinc sulfate is used as the inhibitor,and 2#oil is used as the foaming agent,the molybdenum concentrate with molybdenum grade of 44.938%and recovery rate of 66.54%can be obtained in the laboratory closed-circuit test by using MK-01 as the collector,compared with kerosene as the collector,the molybdenum grade and recovery rate are increased by 0.636 and 2.96 percentage points,respectively.Molybdenum concentrate with molybdenum grade of 42.26%and recovery of 62.71%can be obtained by industrial test.Compared with kerosene as collector,the grade of molybdenum is similar,the recovery rate is increased by 0.72 per-centage point,and the dosage of collector is reduced from 52 g/t to 42 g/t.It shows that the new molybdenum ore collector MK-01 can replace the traditional molybdenum ore collector in Makeng Mining.

molybdenum orecollectoriron tailings

王澜

展开 >

福建马坑矿业股份有限公司

钼矿 捕收剂 选铁尾矿

2024

现代矿业
中钢集团马鞍山矿山研究院有限公司

现代矿业

影响因子:0.33
ISSN:1674-6082
年,卷(期):2024.40(4)
  • 8