现代矿业2024,Vol.40Issue(4) :136-139,143.DOI:10.3969/j.issn.1674-6082.2024.04.031

内蒙古某铁矿石选矿试验研究

Experimental Study on Mineral Processing of an Iron Ore in Inner Mongolia

吴金销 汪劲刚 司晓龙 汪军 高双龙 胡金栓
现代矿业2024,Vol.40Issue(4) :136-139,143.DOI:10.3969/j.issn.1674-6082.2024.04.031

内蒙古某铁矿石选矿试验研究

Experimental Study on Mineral Processing of an Iron Ore in Inner Mongolia

吴金销 1汪劲刚 2司晓龙 1汪军 1高双龙 1胡金栓1
扫码查看

作者信息

  • 1. 中钢天源安徽智能装备股份有限公司
  • 2. 中钢天源股份有限公司
  • 折叠

摘要

为了高效开发利用内蒙古某铁矿石资源,在矿石工艺矿物学性质研究的基础上开展了高压辊磨—湿式磁选抛尾—塔磨—磁选全流程试验研究.结果表明:原矿经高压辊磨制得-1 mm粒级粉矿,在400 mT磁场条件下湿式磁选抛尾,获得了全铁品位36.63%、磁性铁品位为31.31%的湿式预选精矿,湿式预选精矿经塔磨磨至-0.030 mm占95%,经1粗1精磁选获得了铁品位为65.78%、回收率为66.22%的铁精矿,试验结果可以为该铁矿石选别流程确定提供依据.

Abstract

In order to efficiently develop and utilize an iron ore resource in Inner Mongolia,on the ba-sis of the study of the mineralogical properties of ore technology,the whole process of high-pressure roller grinding,wet magnetic separation,tail throwing,tower mill and magnetic separation was carried out.The results show that the-1 mm particle size fine ore was obtained by the high-pressure roller grinding ma-chine,and the wet pre-separation concentrate with a total iron grade of 36.63%and a magnetic iron grade of 31.31%was obtained under the condition of 400 mT,and the wet pre-separation concentrate tower was ground to-0.030 mm accounting for 95%,and the iron concentrate with an iron grade of 65.78%and a re-covery rate of 66.22%was obtained by one roughing and one cleaning magnetic separation,and the test re-sults could provide a feasible process for the iron ore separation.

关键词

铁矿石/粉矿干抛/高压辊磨/塔磨/湿式磁选

Key words

iron ore/dry throwing of powder ore/high pressure roller mill/tower mill/wet magnetic separation