首页|某企业高亚铁含量铁矿粉生产碱性球团焙烧试验

某企业高亚铁含量铁矿粉生产碱性球团焙烧试验

扫码查看
某企业为高效利用高亚铁含量的铁矿粉生产碱性球团,在详细的矿物特性研究的基础上,进行了预热焙烧试验和碱性球团结圈物特性研究.试验结果表明:提高碱度对高亚铁含量铁矿粉生球制备制度及干燥制度影响不明显,适宜的焙烧制度为碱度0.3~1.0,焙烧温度为1 250℃,焙烧时间为 6~10 min,并应避开在碱度0.8时生产球团矿,以避免出现高膨胀率球团;同时提出了应控制铁矿粉SiO2含量及石灰石粉细度,从而抑制回转窑结圈的针对性建议.
Roasting Test of Alkaline Pellets Produced by Iron Ore Powder with High Ferrous Content in an Enterprise
In order to efficiently use the iron ore powder with high ferrous content to produce alkaline pellets,based on the detailed study of mineral characteristics,the preheating roasting test and the character-istics of the alkaline ball solidarity circle are studied.The results show that the increase of basicity has no ob-vious effect on the preparation system and drying system of green pellets of iron ore powder with high ferrous content.The suitable roasting system is that the basicity is 0.3~1.0,the roasting temperature is 1 250℃,and the roasting time is 6~10 min.The pellets produced at the basicity of 0.8 should be avoided to avoid the occurrence of pellets with high expansion rate.At the same time,it is proposed that the SiO2 content of iron ore powder and the fineness of limestone powder should be controlled to inhibit the ring formation of rotary kiln.

high ferrous ironiron ore powderring formationalkalinityreduction expansion

高晓梅

展开 >

太原钢铁(集团)有限公司矿业分公司

高亚铁 铁矿粉 结圈 碱度 还原膨胀

2024