某难选铁矿石全铁品位为32.80%,矿物组成复杂且矿物嵌布粒度微细,为确定后续合理的磨选工艺,进行了选矿工艺试验.试验结果表明:采用阶段磨矿—磁选—淘洗提质工艺,在一段磨矿细度为-74 μm85%,二段磨矿细度为-45 μm75%的条件下,可获得产率为39.47%、铁品位为65.14%、铁回收率为78.38%的铁精矿,尾矿铁品位为11.71%,获得了满意的试验指标.
Separation Process Test of a Low Grade Refractory Iron Ore
The total iron grade of a refractory iron ore is 32.80%.The mineral composition is complex and the particle size of the mineral is fine.In order to determine the subsequent reasonable grinding pro-cess,the beneficiation process test is carried out.The test results show that the iron concentrate with yield of 39.47%,iron grade of 65.14%and iron recovery of 78.38%can be obtained by stage grinding-magnetic sep-aration-elutriation upgrading process under the conditions of grinding fineness of-74 μm 85%in the first stage and grinding fineness of-45 μm 75%in the second stage.The iron grade of tailings is 11.71%.Satisfac-tory test indexes are obtained.

micro-fine refractory iron orestage grindingelutriation and upgrading

唐昊、刘盛辰、李天舒、龙菲菲、李万兴、张轰玉

展开 >

鞍钢集团矿业设计研究院有限公司

微细粒难选铁矿 阶段磨选 淘洗提质

2024

现代矿业
中钢集团马鞍山矿山研究院有限公司

现代矿业

影响因子:0.33
ISSN:1674-6082
年,卷(期):2024.40(11)