为了提高江西某黑钨矿山的钨细泥选矿指标,在钨细泥性质研究的基础上,钨品位0.16%的钨细泥经高梯度磁选1粗1扫分选,再经离心选矿深度精选工艺流程,工业现场应用获得了精矿钨品位0.89%、钨回收率81.56%的选矿指标,实现了较好的分选效果,为后续精选作业创造了有利条件.
Experiment and Application on Recovery of a Wolframite Fine Slime in Jiangxi
In order to improve the beneficiation index of tungsten fine slime in a wolframite mine in Jiangxi Province,based on the study of the properties of tungsten fine slime,the tungsten fine slime with tungsten grade of 0.16%is separated by one roughing and one scavenging high gradient magnetic separa-tion,and then by centrifugal beneficiation process.The beneficiation index of tungsten concentrate with tungsten grade of 0.89%and tungsten recovery of 81.56%is obtained by the industrial field application,which achieved good separation effect and created favorable conditions for subsequent cleaning operations.

wolframite fine slimeSLon magnetic separatorSL centrifugal concentrator

廖国平、钱枝花

展开 >

赣州金环磁选科技装备股份有限公司

磁选设备江西省重点实验室

赣州有色冶金研究所有限公司

黑钨细泥 SLon磁选机 SL离心选矿机