摘要

首先介绍深水导管架项目中马鞍口节点出现的焊接裂纹类型,其次分析裂纹的产生原因,最后针对此类深水导管架项目提出施工过程中的马鞍口焊接节点裂纹预防措施.通过实施全过程质量管理措施,可以有效避免超级延迟裂纹的产生.

Abstract

Firstly,the types of welding cracks in the saddle joint of deep-water jacket projects are introduced,then the causes of cracks are analyzed,and finally the preventive measures for the cracks in the saddle joint during the construction of such deep-water jacket projects are proposed.Through the implementation of the whole process quality control measures,the occurrence of super delayed cracks can be effectively avoided.

关键词

深水导管架/马鞍口/焊接/延迟裂纹/预防措施

Key words

deep water jacket/saddle mouth/welding/delayed crack/preventive measure