扫码查看
以Zn-3Cu合金为研究对象.研究轧制变形量对Zn-3Cu合金的显微组织、力学性能和耐腐蚀性能的影响.结果表明,随着轧制变形量的增加,Zn-3Cu合金基体晶粒细化程度不断加深,合金中的CuZn4相沿着轧制方向不断被拉长并出现部分断裂.Zn-3Cu合金的强度先增后减,塑性不断增强,60%变形量的Zn-3Cu合金具有最高的屈服强度,达到了(263.1±4.9)MPa.随着变形量增加,轧态Zn-3Cu合金的耐腐蚀性能逐渐减弱,铸态Zn-3Cu合金表现出优异的耐腐蚀性能.
Effect of Rolling Deformation on Microstructure,Mechanical Properties and Corrosion Resistance of Zn-3Cu Alloy
The effects of rolling deformation on the microstructure,mechanical properties and corrosion resistance of Zn-3Cu alloy were studied.Results show that with the increase in rolling deformation,the grains of Zn-3Cu alloy matrix are refined,and the CuZn4 phase in the alloy is elongated and partially broken along the rolling direction.The strength of Zn-3Cu alloy increases first and then decreases,and the plasticity increases continuously.The Zn-3Cu alloy with the deformation of 60%has the highest yield strength,reaching(263.1±4.9)MPa.With the increase in deformation,the corrosion resistance of the as-rolled Zn-3Cu alloy gradually decreases,while the as-cast Zn-3Cu alloy exhibits excellent corrosion resistance.

zinc base alloyrolling treatmentmicrostructureperformance

李然然、杨家财、林建国、张德闯

展开 >

湘潭大学材料科学与工程学院,湖南湘潭 411105

锌基合金 轧制处理 组织 性能

国家自然科学基金面上项目

11872053

2024

稀有金属材料与工程
中国有色金属学会,中国材料研究学会,西北有色金属研究院

稀有金属材料与工程

CSTPCD北大核心
影响因子:0.634
ISSN:1002-185X
年,卷(期):2024.53(5)
  • 27