摘要

针对辽宁某低品位金矿合理开发利用,先后对其进行浮选和浸出试验研究,基于本次试验的矿石得到对其进行浸出试验能够获得更好的试验结果.在矿浆浓度 33%、磨矿细度-0.074 mm占 95.05%、CaO用量 1.5 kg/t、无毒浸出剂用量 4.0 kg/t、浸出时间 26h的浸出试验条件下,能获得金、银的浸出率分别为 92.60%和 79.43%较好的选矿指标,为该矿石的合理开发利用提供了理论依据.

Abstract

In order to rationally develop and utilize a low grade gold mine in Liaoning,the flotation and leaching tests were carried out,and the test results obtained from the leaching test of the ore were better.Under the leaching test conditions of grinding fineness of-0.074 mm accounting for 95.05%,calcium oxide dosage of 1.5 kg/t,pulp concentration of 33%,non-toxic leaching agent dos-age of 4.0 kg/t,and leaching time of 26 h,the leaching rates of gold and silver were 92.60% and 79.43% respectively,which pro-vided a theoretical basis for the rational development and utilization of the ore.

关键词

磨矿细度/浮选/浸出

Key words

grinding fineness/flotation/leaching