首页|常温常压下盐酸浸出分离钒钛磁铁精矿中有价金属的试验研究

常温常压下盐酸浸出分离钒钛磁铁精矿中有价金属的试验研究

Research on separation of valuable metals from Panxi iron concentrate by hydrochloric acid leaching at normal temperature and pressure

扫码查看
攀西钒钛磁铁矿组成及矿物结构复杂,难以低成本、高效综合利用其中的有价元素.针对此问题,本文采用常温常压盐酸浸出的方法对该矿物进行了试验探索,考察了盐酸初始质量浓度、浸出液固比、浸出时间、浸出搅拌转速率等主要因素对Fe、TiO2和V2O5浸出率的影响,并通过矿物结构分析了钒钛磁铁精矿中铁、钒、钛分离的机理,得到以下主要结论.盐酸常温常压浸出的较佳工艺条件为盐酸初始浓度20.5%、浸出液固比12:1、浸出时间3.5 h、浸出搅拌转速率600 r/min,该条件下Fe、V2O5和TiO2 浸出率分别为 84.15%、80.80%、10.05%,浸渣中 Fe、V2O5 和 TiO2 品位分别为 26.78%、0.378%和32.58%,实现了钛资源的初步富集;盐酸优先溶解试样中钛磁铁矿矿物的主晶矿物磁铁矿,铁、钒优先进入浸出液,而客晶矿钛铁矿及独立钛铁矿被破坏程度极小,富集于浸渣中;该浸出方法不需要额外的加热和加压设备,具有成本低、能源消耗和设备投资较低、操作简便、环境友好的优势,但浸出指标有待提高,后续需要进一步探索催化剂对常温常压酸浸工艺的影响.
The composition and mineral structure of the Panxi vanadium-titanium magnetite are complex,making it difficult to cost-effectively and efficiently utilize the valuable elements contained within.To address this issue,this paper explores the use of hydrochloric acid leaching at ambient temperature and pressure on the mineral,examining the effects of initial hydrochloric acid concentration,liquid-to-solid ratio,leaching time,and stirring speed on the leaching rates of Fe,TiO2,and V2O5.Additionally,the paper analyzes the mechanism of separation of iron,vanadium,and titanium in the vanadium-titanium magnetite concentrate through mineral structural analysis,reaching the following main conclusions.The optimal process conditions for hydrochloric acid leaching at ambient temperature and pressure are an initial hydrochloric acid concentration of 20.5%,a liquid-to-solid ratio of 12:1,a leaching time of 3.5 hours,and a stirring speed of 600 rpm.Under these conditions,the leaching rates of Fe,V2O5,and TiO2 are 84.15%,80.80%,and 10.05%,respectively.The concentrate in the leach residue contains 26.78%Fe,0.378%V2O5,and 32.58%TiO2,achieving preliminary enrichment of titanium resources.The hydrochloric acid preferentially dissolves the main crystal mineral magnetite in the titanomagnetite mineral,with iron and vanadium preferentially entering the leach solution,while the guest crystal mineral ilmenite and independent ilmenite are minimally disrupted and enriched in the leach residue.This leaching method does not require additional heating or pressurization equipment,offering advantages such as low cost,low energy consumption and equipment investment,simplicity of operation,and environmental friendliness.However,the leaching indicators still need to be improved,and further exploration of the impact of catalysts on the ambient temperature and pressure acid leaching process is needed in the future.

vanadium-titanium magnetiteseparation of iron,vanadium and titaniumhydrochloric acid leachingnormal temperature and pressuremineral structurecatalyst

徐国印、王普蓉、张翠平、马兰

展开 >

攀枝花学院,四川攀枝花 617000

钒钛资源综合利用四川省重点实验室,四川攀枝花 617000

国家钒钛检测重点实验室,四川攀枝花 617000

钒钛磁铁矿 铁、钒、钛分离 盐酸浸出 常温常压 矿物结构 催化剂