首页|TC4钛合金短电弧钻孔工艺性能研究

TC4钛合金短电弧钻孔工艺性能研究

扫码查看
为了提高小孔钻削的加工效率和尺寸精度,文章提出了一种新颖高效的管电极短电弧钻孔方法.然而,由于电弧放电能量过大与进给速度不匹配,使得高效、高尺寸精度的小孔加工困难重重.文章揭示了基于脉冲电源的短电弧钻孔的工作原理,分析了SEAD的电压电流波形和截面形貌.此外,还研究了不同电极极性、电压、脉冲频率、占空比和电极进给速率对材料去除率(MRR)、电极相对磨损比(REWR)、平均直径和锥度的影响.最后,通过工艺参数优化实验,得到了小孔SEAD参数的最优组合,验证了小孔SEAD的加工性能.实验结果表明,在最佳加工参数下,小孔SEAD的材料去除率最高,为 84.51 μm/s,电极相对磨损比较低,为 29.34%.加工小孔的最小平均直径和锥度分别为 698.49 μm和 0.001 1°.
Research on the performance of short electric arc drilling process of TC4 titanium alloy
To improve the machining efficiency and dimensional accuracy of small hole drilling,a novel and efficient method of small hole short electric arc drilling(SEAD)by tube electrode is proposed.However,due to the mismatch between excessive arc discharge energy and feed rate,efficient and high dimensional accuracy small hole machining is fraught with difficulties.This paper reveals the mechanism of SEAD based on pulsed power supply,and analyzes the voltage-current waveform and cross-section topography of SEAD.In addition,the influence of different electrode polarity,voltage,pulse frequency,duty cycle,and electrode feed rate on material removal rate(MRR),relative electrode wear ratio(REWR),average diameter,and taper were investigated.Finally,an optimum combination of small hole SEAD parameters was obtained through a process parameter optimization experiment,which confirmed the machining performance of small hole SEAD.The experimental results show that under the optimal machining parameters,small hole SEAD achieves the highest MRR of 84.51 μm/s and a relatively low REWR of 29.34%.The minimum average diameter and taper of the machined small hole were 698.49 μm and 0.001 1°,respectively.

short electric arc drillingarc dischargematerial removal raterelative electrode wear ratioaverage diametertaper

付斐、胡国玉、张晟晟、王家豪、周建平

展开 >

新疆大学智能制造现代产业学院,新疆 乌鲁木齐 830047

短电弧钻孔 电弧放电 材料去除率 电极相对磨损比 平均直径 锥度

国家自然科学基金

52265060

2024

制造技术与机床
中国机械工程学会 北京机床研究所

制造技术与机床

CSTPCD北大核心
影响因子:0.264
ISSN:1005-2402