首页|Fe-Mo-B Enhanced Sintering of P/M 316L Stainless Steel

Fe-Mo-B Enhanced Sintering of P/M 316L Stainless Steel

扫码查看
Liquid-phase enhanced sintering of powder metallurgy (P/M) 316L stainless steel by addition of sintering aids was studied. 2% - 8% of pre-alloyed Fe-Mo-B powder with two different particle sizes was added as sintering aids, and the specimens were sintered in vacuum at 1 200 - 1 350 ℃. The results show that the fine Fe-Mo-B powder (5 - 10 μm) has stronger activated effect. The sintered density increases with the increase in sintering aid content or sintering temperature. Warm compaction has a better effect on the control of dimensional precision of compacts. The prealloyed Fe-Mo-B powder deviated from Mo_2FeB_2 component can also be sintering aid of P/M 316L stainless steel.

YANG Xia、GUO Shi-ju

展开 >

2008

Journal of iron and steel research international

Journal of iron and steel research international

EIISTP
ISSN:1006-706X
年,卷(期):2008.15(1)