首页|On the Firing Test Properties of Thinfilm Metallic Initiators

On the Firing Test Properties of Thinfilm Metallic Initiators

扫码查看
The aim of this study was to investigate the firing test properties of NiCr alloy thin film bridge electro-initiators(detonators). The function time of firing test was characterized in terms of their area, shape, resistance, and thickness of thin film bridge electro-initiators(detonators). It is found that samples with small film bridge area show profound and positive influence on the function time of firing test. The shortest function time is 120 μs (3.165 Ω).