Trans Tech Publications Ltd
Single crystals of x (Bi_(0.5)K_(0.5))TiO_3-(1-x)(Bi_(0.5)Na_(0.5))TiO_3 (BKT-BNT) solid solution were grown by a flux method, and their ferroelectric properties were investigated along [100]_(cubic) (the cubic notation). While the flux growth soaked at 1250 ℃ led to the crystals with a composition of x less than 0.14, the crystals with x of 0.45 were obtained by decreasing soaking temperature to 1150 ℃. The crystals of BKT-BNT (x = 0.45) exhibited a relatively large remanent polarization of 39 μC/cm~2 and a low coercive field of 23 kV/cm.