La2O3在钼中可以细化晶粒尺寸,钉扎位错,提高钼的强度.铼可以降低钼的塑脆转变温度,提高强度和延伸性能.为了充分发挥La2O3的细晶强化作用,进一步提升MR14板材的性能,通过固固掺杂、固液还原掺杂和液液掺杂三种混粉工艺,研究了 La2O3掺杂方式对MR14合金的性能影响.研究表明,固液还原掺杂和液液掺杂两种混粉方式,均可以细化晶粒,提高显微硬度和室温力学性能,且性能差异较小,伸长率比固固掺杂的板坯高50%.
Effect of La2O3 doping methods on the properties of MR14 plates
La2O3can refine grain size,pin dislocations,and improve the strength of molybdenum.Rhenium can re-duce the ductile brittle transition temperature of molybdenum,improve its strength and elongation performance.In order to fully utilize the fine grain strengthening effect of La2O3 and further improve the mechanical properties of MR 14 sheet,this article studied the effect of La2O3 doping methods on the properties of MR 14 alloy through three powder mixing processes:solid solid doping,solid liquid reduction doping,and liquid liquid doping.Research has shown that both solid-liquid reduction doping and liquid-liquid doping can refine grain size,improve microhard-ness and room temperature mechanical properties,with small performance differences and a 50%higher elongation than solid-liquid doped plates.

molybdenum-rhenium alloyrare earth oxidedoping methodmicrostructuremechanical property

王广达、张丹华、熊宁、况春江

展开 >

钢铁研究总院有限公司,北京 100081

安泰科技股份有限公司,北京 100081

钼铼合金 稀土氧化物 掺杂工艺 微观组织 力学性能

国家重点研发计划专项资助项目

2022YFB3705400

2024

粉末冶金工业
中国钢研科技集团有限公司 中国钢协粉末冶金分会 中国机协粉末冶金分会

粉末冶金工业

CSTPCD北大核心
影响因子:0.406
ISSN:1006-6543
年,卷(期):2024.34(2)
  • 34