首页|压缩籽棉对棉籽破碎率及纤维品质的影响

压缩籽棉对棉籽破碎率及纤维品质的影响

扫码查看
为探究压缩对籽棉品质的影响因素与规律,以含水率、含杂率及压缩密度为试验因素,以棉籽破碎率、纤维长度、马克隆值、伸长率、反射率、黄度、整齐度、纤维强度为指标进行研究.结果表明:含水率、含杂率及压缩密度对棉籽破碎率影响显著(P<0.05),棉籽破碎率随压缩密度增大而增大,随含水率增加而降低;压缩密度仅对棉籽破碎率和反射率有显著影响(P<0.05);纤维长度随压缩密度、含水率增加而增加,随含杂率增加而减小;马克隆值随含杂率及含水率增加而增加,随压缩密度增加而减小;伸长率随含杂率增加而增加,随压缩密度及含水率增加而减小;反射率随压缩密度增大而增大,随含杂率增大而减小;黄度随含杂率增加而降低,随含水率增大而增大.
Effect of compression parameters on cottonseed crushing rate and cotton fiber quality
Objective Machine-harvested seed cotton always undergoes compression and baling procedure to augment fiber packing density and diminish volume,thereby enhancing the efficiency of cotton transportation and storage.However,determining an optimal range for compression parameters,then ensuring minimal damage to the cottonseed and maximal preservation of cotton fiber quality,holds significant importance for cotton production.Therefore,it is imperative to investigate the morphology of the compressed cottonseed and the cotton fiber quality.Method To determine the primary and secondary relationship and the influence law of the compression parameters on the seed cotton quality,this study took the moisture content,trash content and compression density as the factors,and the cotton seed crushing rate,fiber length,micronaire value,elongation,reflectance(Rd),yellowness(+b),uniformity,and fiber strength as the indexes.Machine-harvested seed cotton was obtained through the cotton picking performance test,the cotton was compressed through the compression equipment,and the compressed cottonseeds and cotton fibers were obtained through ginning.The compressed cottonseed was chemically defluffed and dried to obtain the polished cottonseed,which was observed and screened with a microscope to obtain the cottonseed crushing rate;the compressed cotton fiber was sent to the testing laboratory to obtain the cotton fiber quality test results.Results The results of variance analysis indicate that the order of the affecting factors of the crushing rate of cottonseed after compression is compression density,moisture content,and trash content.The order for fiber length is trash content,moisture content,and compression density.The order for micronaire value is moisture content,trash content,and compression density.The order for the elongation was moisture content,trash content,and compression density.The order for reflectivity was moisture content,trash content,and compression density.The order for yellowness was trash content,moisture content,and compression density.The order for uniformity was trash content,compression density,and moisture content.The order for fiber strength was compression density,trash content,and moisture content.The effect of moisture content,trash content,and compression density on cotton seed crushing rate was significant(P<0.05).The cotton seed crushing rate increased with increasing compression density,and decreased with in-creasing moisture content at a higher compression density.Trash content had no significant effect(P>0.05)on uniformity,fiber strength,elongation,reflectance.And compression density only had a significant effect(P<0.05)on cottonseed crushing rate and reflectance.Fiber length increased with increasing compression density and increasing moisture content,but decreased with increasing trash content.The micronaire value increased with the increase of trash content,decreased with the increase of compression density,and increased with the increase of moisture content.Elongation increased with increasing trash content,decreased with increasing compression density,and decreased slowly with increasing moisture content.The reflection rate increased with increasing compression density and decreased with increasing moisture content.The cottonseed crushing rate is the smallest when the moisture content is 14%,the trash content is 16%,and the compression density is 200 kg/m3.The maximum fiber length is obtained when the moisture content is 14%,the trash content is 8%and the compression density is 400 kg/m3.The elongation is minimized when the moisture content is 14%,the trash content is 8%,and the compression density is 400 kg/m3.The reflectance is minimized when the moisture content is 14%,the trash content is 8%,and the compression density is 200 kg/m3.The minimum yellowness is obtained when the moisture content is 6%,the trash content is 16%,and the compression density is 200 kg/m3.The micronaire value is between 4.50 and 4.90,which is at the standard level.Conclusion Finally,we obtained that under the premise of ensuring higher compression density,increasing moisture content and trash content can ensure a smaller cotton seed crushing rate,while increasing moisture content will lead to a decrease in elongation,and increasing trash content will reduce fiber length and increase reflectivity.The research results have certain theoretical value for the determination of the working conditions of cotton picker and the design and selection of the parameters of compression molding device of cotton picker.

fiber qualitycottonseed crushing ratecompression densitymoisture contenttrash contentmachine-harvested seed cotton

魏喜梅、张莹洁、张宏文、王军、王蒙

展开 >

石河子大学机械电气工程学院,新疆石河子 832000

南京师范大学电气与自动化工程学院,江苏南京 210023

石河子大学农业农村部西北农业装备重点实验室,新疆石河子 832000

石河子大学棉花生产技术现代化省部共建协同创新中心,新疆石河子 832000

展开 >

纤维品质 棉籽破碎率 压缩密度 含水率 含杂率 机采籽棉

国家自然科学基金项目兵团重点领域创新团队建设项目石河子大学青年创新人才计划项目

322604352019CB006CXPY202120

2024

纺织学报
中国纺织工程学会

纺织学报

CSTPCD北大核心
影响因子:0.699
ISSN:0253-9721
年,卷(期):2024.45(10)