首页|钙处理工艺对耐腐蚀船板钢低温韧性的影响

钙处理工艺对耐腐蚀船板钢低温韧性的影响

扫码查看
针对高强度耐腐蚀船板钢的低温冲击韧性波动范围大,低温冲击韧性低这一生产中亟待解决的问题.研究了钙处理工艺对高强度耐腐蚀船板钢低温冲击性能的影响,与传统的钙处理工艺相比,改进后的钙处理工艺能较大提高试验钢的-20℃和-40℃的低温冲击性能.当夹杂物为球形钙铝酸盐+CaS的复合夹杂物且弥散分布时,试验钢的-20℃冲击功横向提高了24.6%,纵向提高了44.5%:-40℃冲击功横向提高了33.7%,纵向提高了32.7%.改进后的钙处理工艺,提高了钢水中[Ca]的收得率,使钙处理更充分,从而得到了低温冲击性能稳定且优良的试验钢板.
Effect of Calcium Treatment on Low Temperature Toughness of Corrosion Resistant Steel
In order to stabilize the low temperature toughness of corrosion resistant steel,effect of calcium treatment on low temperature toughness of corrosion resistant steel has been studied.The results show that compared with the traditional calcium treatment process,the modified calcium treatment process can greatly improve the low temperature impact properties of steel tested at the temperature of-20 ℃ and-40 ℃.When the inclusions are spherical calcium aluminate +CaS composite inclusions and dispersed,the test steel at-20 ℃ impact energy (transverse) was improved by 24.6%,and the value at-40 ℃ impact energy (transverse) was improved by 44.5%,and the impact values the sample along longitudinal direction was improved by 33.7% and 32.7% respectively.The modified calcium treatment technology can improve the absorption rate of [Ca] in the molten steel which makes it more effective and a steel plate of with satisfied low temperature impact toughness was obtained.

corrosion resistant steelcalcium treatmentimpact toughnessinclusions

吴战芳、徐李军、董富军、仇圣桃、李向阳

展开 >

钢铁研究总院连铸技术国家工程研究中心,北京100081

东北大学材料与冶金学院,辽宁沈阳110004

新余钢铁有限责任公司,江西新余338001

中国钢研科技集团有限公司,北京100081

展开 >

耐腐蚀船板钢 钙处理 冲击韧性 夹杂物

2016

钢铁钒钛
攀钢集团攀枝花钢铁研究院有限公司

钢铁钒钛

CSTPCD北大核心
影响因子:0.395
ISSN:1004-7638
年,卷(期):2016.37(4)
  • 4
  • 4