首页|半自磨机用Fe-1.1C-20Mn-2.5Cr-0.9Si-0.25Ti-1.0V-0.15Nb衬板的失效分析

半自磨机用Fe-1.1C-20Mn-2.5Cr-0.9Si-0.25Ti-1.0V-0.15Nb衬板的失效分析

扫码查看
针对某选矿厂∅10.37 m×5.49 m半自磨机高锰钢衬板在使用过程中出现断裂的情况,采用X射线荧光光谱仪(XRF)、扫描电子显微镜(SEM)和电子试验机(AGS-X 100KNx)等设备对衬板的化学成分、微观组织和拉伸断口形貌进行分析.结果表明衬板中存在疏松以及晶界处大量未溶块状碳化物和网状碳化物是导致半自磨机衬板早期断裂的主要原因.
Failure Analysis of Fe-1.1C-20Mn-2.5Cr-0.9Si-0.25Ti-1.0V-0.15Nb Lining Plant for Semi-self-grinding Machine
In order to find out the fracture cause of the high-manganese steel lining plate for ∅10.37m × 5.49 m semi-self-grinding machine for a mineral processing plant,the X-ray fluorescence spectrometer(XRF),scanning electron microscopy(SEM),electronic testing machine(AGS-X 100KNx)and other devices were used to analyze the chemical composition,microstructure and fracture morphology of the lining plate.The results showed that the main reasons for early fracture of the lining plate for semi-self-grinding machine were the looseness in the lining plate,and the large number of undissolved block carbides and network carbides at the grain boundary.

high manganese steelloosenesscarbidesfracture

王栋栋、王彬、汪军

展开 >

铜陵有色金神耐磨材料有限责任公司,安徽铜陵 244000

高锰钢 疏松 碳化物 断裂

安徽省科技重大专项

202103a05020002

2024

热处理技术与装备
江西省科学院应用物理研究所 中国热处理行业协会

热处理技术与装备

影响因子:0.3
ISSN:1673-4971
年,卷(期):2024.45(2)
  • 18