首页|光固化3D打印光敏树脂的临界能量和固化深度影响因素

光固化3D打印光敏树脂的临界能量和固化深度影响因素

扫码查看
不同的3D打印光敏树脂,在同一3D打印机下进行光固化,其固化性能有所差异.采用临界曝光量和固化深度2个特性参数来表征光固化树脂的光敏性,探讨了临界曝光量和固化深度之间的数学关系,研究了临界曝光量和固化深度的测定方法,测定了光强和树脂的颜色对树脂固化的影响.在一定条件下,固化深度通常随光照强度的增加而增加,临界曝光量也随光照强度的增加而增加;浅色比深色树脂固化深度高,且所需临界曝光量更高.同时,固化深度随着光引发剂的浓度增加而降低;临界曝光量随着光引发剂浓度的增加先降低,后趋于平缓.
Studies on the influence factors on Ec and Dp of photocuring 3D printing photosensitive resin
The curing performance of different 3D printing photosensitive resins varies,which are light cured under the same 3D printer.2 characteristic parameters,critical exposure and transmission depth,were used to characterize the photosensitivity of photosensitive adhesives,and the mathematical relationship between critical exposure and transmission depth was explored.The measuring methods of critical exposure and penetration depth were studied.The effects of light intensity and resin color on resin curing were measured.Under certain conditions,the penetration depth generally increased with the increase of light intensity,and the critical exposure also increased with the increase of light intensity.Light colors have higher penetration depth than dark colors,and require higher critical exposure.The depth of cure decreases with increasing concentration of photoinitiator.The critical exposure decreases firstly with the increase of photoinitiator concentration,and then tends to be flat.

3DPresinpenetration depthcritical exposure

陈静、杨晓帅、张鹏飞、张爱平

展开 >

河南省能碳研究院有限公司,郑州 450000

3D打印 树脂 固化深度 临界曝光量

2024

科技导报
中国科学技术协会

科技导报

CSTPCD北大核心
影响因子:0.559
ISSN:1000-7857
年,卷(期):2024.42(4)
  • 12