CoNiCrAlY涂层常用作工作层和金属基体之间的过渡层.采用了SHV-50 超音速火焰喷涂设备在 45 钢表面制备了CoNiCrAlY涂层.分析了CoNiCrAlY涂层的微观组织结构、显微硬度、孔隙率、表面粗糙度、结合强度、电化学性能.结果表明:SHV-50 超音速火焰喷涂获得的CoNiCrAlY涂层的孔隙率为 0.48%,涂层的平均显微硬度为 497.2 HV0.2,涂层结合强度均值达 70 MPa,抗热震次数达 26 次,涂层的表面粗糙度平均值为Ra6.43,利于工作层与过渡层的结合.CoNiCrAlY涂层的抗电化学腐蚀能力强于基体.SHV-50 超音速火焰喷涂设备制备的CoNiCrAlY涂层可用作工作层和金属基体之间的过渡层.
Study on Properties of CoNiCrAlY Coating Prepared by Supersonic Flame Spraying
CoNiCrAlY coating was used as a transition coating between working coatings and metal matrix.The CoNiCrAlY coating was sprayed on 45 steel surface by SHV-50 supersonic flame spraying equipment.The microstructure,microhardness,porosity,surface roughness,bonding strength and electrochemical properties of the CoNiCrAlY coatings were characterized.The results show that the porosity of the CoNiCrAlY coating obtained by SHV-50 supersonic flame spraying is 0.48%,the average microhardness of the coating is 497.2 HV0.2.The average bounding strength of the coating is 70 MPa.The number of thermal shocks up to 26 times.The surface roughness of the coating is Ra6.43,which is better for the combination of surface layer and transition layer.CoNiCrAlY coating has stronger electrochemical corrosion resistance than matrix.So CoNiCrAlY coatings sprayed by SHV-50 supersonic flame spraying equipment can be used as transition layers between working coatings and metal substrates.

supersonic flame sprayingCoNiCrAlYtransition layerbonding strength

伏利、陈小明、赵坚、刘伟

展开 >

水利部产品质量标准研究所,浙江 杭州 310012

浙江省水利水电装备表面工程技术研究重点实验室,浙江 杭州 310012

水利部杭州机械设计研究所,浙江 杭州 310012

超音速火焰喷涂 CoNiCrAlY 过渡层 结合强度

浙江省科技计划杭州市科技发展计划浙江省科技计划

2016C3709120162231E102018C37029

2024

热加工工艺
中国船舶重工集团公司热加工工艺研究所 中国造船工程学会船舶材料学术委员会

热加工工艺

CSTPCD北大核心
影响因子:0.55
ISSN:1001-3814
年,卷(期):2024.53(7)
  • 16