为改善水泥稳定碎石力学及耐久性能,研究了不同PVA纤维长度与掺量下水泥稳定碎石系列力学性能,确定了 PVA纤维最佳掺配长度及掺量.在此基础上,借助冻融循环与疲劳试验,研究了普通水泥稳定碎石与PVA纤维水泥稳定碎石耐久性能差异.结果表明:随着PV A纤维长度或掺量的增大,PVA纤维水泥稳定碎石系列力学性能均先增大后减小;长度12 mm、掺量0.9 kg/m3的PVA纤维水泥稳定碎石综合性能最佳;28 d龄期时,在冻融5、10、15次后,长度12 mm、掺量0.9 kg/m3的PVA纤维水泥稳定碎石抗压强度保持率为90.21%~84.39%;长度12 mm、掺量0.9 kg/m3的PVA纤维水泥稳定碎石在应力强度比为0.7~0.8下,疲劳寿命提升了 135.29%~175.01%.
To improve the mechanical and durability properties of cement stabilized-macadam,the evolution law of series mechanical properties of cement stabilized-macadam with different PVA fi-ber length and dosage were investigated,and the optimum length and dosage of PVA fiber were de-termined.On this basis,the difference in durability between ordinary cement-stabilized macadam and PVA fiber cement-stabilized macadam was studied by means of freeze-thaw cycle and fatigue test.The results show that the series mechanical properties of PVA fiber cement stabilized-macadam increase and then decrease with the increase of PVA fiber length or dosage.Compared with the oth-er test schemes,the comprehensive performance of PVA fiber cement stabilized-macadam with 12 mm length and 0.9 kg/m3 dosage is the best.At 28 d,after 5,10 and 15 freeze-thaw cycles,the compressive strength retention rate of PVA fiber cement stabilized-macadam with 12 mm length and 0.9 kg/m3 dosage is 90.21%~84.39%.The fatigue life of PVA fiber cement stabilized-macadam with 12 mm length and 0.9 kg/m3 dosage increases by 135.29%~175.01%under 0.7~0.8 stress intensity ratio.

road engineeringPVA fibercement stabilized-macadammechanical propertydurability

冯仲文

展开 >

中铁十八局集团第五工程有限公司,天津 300453

道路工程 PVA纤维 水泥稳定碎石 力学性能 耐久性能

国家自然科学基金面上项目

52378252

2024

沈阳理工大学学报
沈阳理工大学

沈阳理工大学学报

影响因子:0.223
ISSN:1003-1251
年,卷(期):2024.43(6)