以次甲基蓝作为预还原指示剂,建立了氯化亚锡还原,重铬酸钾无汞滴定铁矿石中全铁的分析方法.探讨了方法的基本原理和测定条件,并试验了预还原反应指示剂用量对分析结果的影响.结果表明:以SnCl2为预还原剂,次甲基蓝为预还原指示剂时,滴加2~3滴浓度为2.94 g/L的次甲基蓝,预还原终点和滴定终点颜色变化敏锐.干扰试验表明铁矿石中大多数元素均不干扰测定.对两种铁矿石进行分析,测定结果的相对标准偏差(RSD)分别为0.34%和0.16%.利用标准方法进行对照试验,发现在95%的置信度下,两种方法所得到的测定值其精密度无显著性差异,两组数据的平均值之间也无显著性差异.
Determination of total iron in iron ore by stannous chloride-methylene blue-potassium dichromate mercury-free titration
A method for determining total iron in iron ore by potassium dichromate mercury-free titration was established by using methylene blue as pre-reduction indicator and stannous chloride as reduction agent.The fundamental principle and testing condition of the testing method was discussed and the effect of the dosage of pre-reduction reaction indicator on testing result was tested.The result indicated the color change of pre-reduction terminal and titration end point was acute by using SnC12 as pre-reduction agent, methylene blue as pre-reduction indicator and adding 2-3 drops of 2.94 g/L methylene blue.The interference test indicated most elements in iron ore did not interfere with the test.Analysis was conducted on two types of iron ore, with RSD of 0.34% and 0.16% respectively.Control test was conducted by standard method.It was found under the confidence level of 95 %, no significant difference was found on the precision of the test results of both methods.No significant differences were found between the average values of both data as well.

methylene bluestannous chloridepotassium dichromate mercury-free titrationiron oretotal iron

谢岁强、胡秀艳、李晓燕、唐星星

展开 >

乐山师范学院化学学院,四川乐山614000

次甲基蓝 氯化亚锡 重铬酸钾无汞滴定法 铁矿石 全铁

乐山师范学院教改重点项目

JC10-ZD08

2013

冶金分析
中国钢研科技集团有限公司(钢铁研究总院) 中国金属学会

冶金分析

CSTPCDCSCD北大核心
影响因子:1.124
ISSN:1000-7571
年,卷(期):2013.33(4)
  • 14
  • 8